+高级检索
晶粒结构对变形Mg-0.8Bi-0.35Al-0.35Ge合金力学性能及腐蚀行为的影响
作者:
作者单位:

1.太原理工大学 材料科学与工程学院,山西 太原 030024;2.孝义市东义镁业有限公司,山西 孝义 032308;3.河北工业大学 材料科学与工程学院,天津 300132

作者简介:

通讯作者:

中图分类号:

TG146.22

基金项目:

山西省自然科学基金(202103021224049);吕梁市校地合作重点研发专项(2023XDHZ09)


Effect of Grain Structure on Mechanical Properties and Corrosion Behavior of Deformed Mg-0.8Bi-0.35Al-0.35Ge Alloys
Author:
Affiliation:

1.College of Materials Science and Engineering, Taiyuan University of Technology, Taiyuan 030024, China;2.Xiaoyi Dongyi Magnesium Industry Co., Ltd, Xiaoyi 032308, China;3.School of Materials Science and Engineering, Hebei University of Technology, Tianjin 300132, China

Fund Project:

Natural Science Foundation of Shanxi (No. 202103021224049), Lvliang City University-local Government Cooperation key research and development project (No. 2023XDHZ09)

  • 摘要
  • |
  • 图/表
  • |
  • 访问统计
  • |
  • 参考文献
  • |
  • 相似文献
  • |
  • 引证文献
  • |
  • 资源附件
  • |
  • 文章评论
    摘要:

    通过轧制和挤压工艺制备了具有不同晶粒结构的Mg-0.8Bi-0.35Al-0.35Ge合金,包括均质结构的E-T2合金和异质结构的R-T2合金,探讨了晶粒结构对变形合金力学性能及腐蚀行为的影响。结果表明,E-T2合金展现出均质等轴晶组织,而R-T2合金则表现出项链状的双峰晶粒结构。E-T2合金具有较好的力学性能和耐腐蚀性能协同效果,其屈服强度为208.0 MPa,抗拉伸强度为274.0 MPa,延伸率为25.4%,腐蚀速率为0.12 mm/a。相比之下,R-T2合金虽然屈服强度更高(285.0 MPa),但其耐腐蚀性能较差(腐蚀速率为0.35 mm/a),这主要和晶界处存在的阴极相Mg3Bi2和高密度位错导致的严重晶间腐蚀有关。

    Abstract:

    Mg-0.8Bi-0.35Al-0.35Ge alloys with different grain structures were prepared by rolling and extrusion processes, including homogeneous E-T2 alloy and heterogeneous R-T2 alloy. The effects of grain structure on the mechanical properties and corrosion behavior of deformed alloys were discussed. Results show that the E-T2 alloy exhibits a homogeneous equiaxed grain structure, whereas the R-T2 alloy exhibits a necklace bimodal grain structure. E-T2 alloy exhibits excellent mechanical properties with synergistic corrosion resistance, whose yield strength, ultimate tensile strength, elongation, and corrosion rate are 208.0 MPa, 274.0 MPa, 25.4%, and 0.12 mm/a, respectively. In contrast, although R-T2 alloy has higher yield strength (285.0 MPa), its corrosion resistance is inferior (0.35 mm/a). This is mainly related to the severe intergranular corrosion caused by the presence of cathode Mg3Bi2 phase and high-density dislocations at the grain boundary.

    参考文献
    相似文献
    引证文献
引用本文

巩珊珊,程伟丽,张全福,宋蕾,曹继栓,余晖.晶粒结构对变形Mg-0.8Bi-0.35Al-0.35Ge合金力学性能及腐蚀行为的影响[J].稀有金属材料与工程,2025,54(6):1603~1612.[Gong Shanshan, Cheng Weili, Zhang Quanfu, Song Lei, Cao Jishuan, Yu Hui. Effect of Grain Structure on Mechanical Properties and Corrosion Behavior of Deformed Mg-0.8Bi-0.35Al-0.35Ge Alloys[J]. Rare Metal Materials and Engineering,2025,54(6):1603~1612.]
DOI:10.12442/j. issn.1002-185X.20240673

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2024-10-16
  • 最后修改日期:2024-12-27
  • 录用日期:2025-01-03
  • 在线发布日期: 2025-06-10
  • 出版日期: 2025-06-09