    摘要:

    基于EET理论,计算了a-Al与S相及S/a相界面的价电子结构,分析了S相价电子结构与析出强化、S/a相界面价电子结构与界面性能的关系。研究表明:S相共价键分布较为均匀,Cu原子将S相原子间键合力最强的4条共价键连接在一起构成主键络。S相析出强化的微观本质在于其最强共价键的键合力比基体a-Al的大135.14%,对位错运动具有较强的阻力作用。S相与基体a-Al形成的(100)S//(100)a和(010)S// a及(001)S//(021)a面的共价电子密度差Dr分别为0.003%、3.564%和5.811%,(100)S//(100)a面上的共价电子密度为10.3915 nm-2和10.3918 nm-2,(010)S// a面上的共价电子密度为0.0486 nm-2和0.0469 nm-2,(001)S//(021)a面上的共价电子密度为0.0486 nm-2和0.0459 nm-2。与(001)S//(021)a和(010)S// a面相比,(100)S//(100)a面的原子键合力与共价电子密度均最大,共价电子密度差最小,界面连续性最好,界面的应力最小。

    Abstract:

    Based on the empirical electron theory of solids and molecules, the valence electron structures of S phase and the S/a interface were calculated, then the relationships between their VESs and precipitation strength and interface properties were analyzed in Al-Cu-Mg alloys in this paper. It is shown the covalent bond distribution of S phase is uniform and its main bond network is built by four stronger covalent bonds connected by Cu atoms. The nature of precipitation strength of S phase lies in its binding force of the strongest covalent bond is bigger 135.14% than that of the matrix a-Al and causes the stronger inhibition to the dislocation movement. The covalent electron density difference of (100)S//(100)a, (010)S// aand (001)S//(021)ais 0.003%, 3.564%and 5.811% respectively, while the covalent electron density of (100)S//(100)ais 10.3915 nm-2 and 10.3918 nm-2 , and that of (010)S// ais 0.0486 nm-2 and 0.0469 nm-2, and that of (001)S//(021)ais 0.0486 nm-2 and 0.0459 nm-2. Compared with (001)S//(021)a和(010)S// a, the binding force and covalent electron density of (100)S//(100)a is the biggest while its covalent electron density difference is the smallest, so that the interface continuity is the best and the interface stress is the smallest.

    参考文献
    相似文献
    引证文献
引用本文

屈华,徐巧至,刘伟东,齐健学. Al-Cu-Mg合金S相及S/a相界面价电子结构分析[J].稀有金属材料与工程,2020,49(11):3816~3821.[Qu Hua, Xu Qiaozhi, Liu Weidong, Qi Jianxue. Valence electron structures analysis of S phase and the S/a interface in Al-Cu-Mg alloy[J]. Rare Metal Materials and Engineering,2020,49(11):3816~3821.]
DOI:[doi]

复制
文章指标
  • 点击次数:
  • 下载次数:
  • HTML阅读次数:
  • 引用次数:
历史
  • 收稿日期:2020-04-22
  • 最后修改日期:2020-05-09
  • 录用日期:2020-05-27
  • 在线发布日期: 2020-12-09
  • 出版日期: